Sandy Bottom Anchor Tests Anchor tests were conduced on February 17-18, 1990 by NAV-X Corporation of Ft. Lauderdale, FL, manufacturers of FORTRESS Marine Anchors. All tests and procedures were verified by the Author of "Chapman's Piloting * Seamanship," Elbert S. Maloney. The tests were also witnessed in part by invited members of the marine industry, including Paul Thompson and Bill Glass of Simpson Lawrence, Ltd., manufacturers of the "CQR," "Delta," and "Harborfast" anchors. The tests were also witnessed at various times by editorial representatives of the following marine publications: Burleigh Magazines, Ltd. (UK), Cruising World/Sailing World Magazines, Motor Boating & Sailing, Multihulls Magazine, Power & Motoryacht, Practical Sailor, Sail, and Yachting Magazine. A photographic and videotape record of the tests was obtained. PURPOSE: DESCRIPTION OF THE TEST SITE TEST VESSELS SCOPE AND ANCHOR RODE 6 lengths of 1-1/4" three strand nylon line were precut with thimbles spliced into each end for testing. The finished lengths of 95' each, when coupled to a 6' length of 1/2" high test (Grade 40) chain, were designed to provide a scope of 5 to 1 in this particular anchorage, as measured from the tug's deck to the sea bottom. (5' + 15' = 20' X 5=100'). For safety during the maximum pull test on the 65lb FORTRESS FX-125, a larger length of 1-1/2" line was added to insure that the weaker 1-1/2" line would be entirely below water, which would absorb the rope's stored energy should the line break during testing at loads approaching 20,000 lbs. (Such a break did occur during a pull of the FORTRESS FX-125). The diameters of the rope and chain used was larger than that normally specified for use with anchors of the main size category. The larger size was chosen for safety during testing. LOAD MEASURING Test loads were measured on two calibrated "Dillon" analog dynometers, each having a certificate of accuracy traceable to the U.S. Bureau of Standards. The first, which measures loads from 0-10,000 lbs (12,000 maximum), was used for all anchors except the larger FORTRESS FX-85/125. for which the larger 0-20,000 lb. unit was sometimes used. ANCHORS TESTED 10 anchors in all were tested and are described and illustrated below. Actual weight varied from 19 lbs. to 65 lbs. Generally, the test involved anchors in the 35-40 pounds steel "Danforth Type" size class. This size class was selected for testing because it represents the size often chosen for service aboard cruising boats in the 35' to 50' class. Generally speaking, a given anchor's "performance ratio" or holding power per pound of anchor weight, can be used to determine the performance that can be expected from different sizes of the same model and design. All anchors, including the FORTRESS models, were purchased by NAV-X Corporation, and chosen randomly from the stocks of local retailers and distributors (Sailorman, and Lewis Marine Supply, Ft. Lauderdale, FL). AL anchors were inspected prior to testing, and found to be generally within their manufacturer's advertised specifications, except where noted below. PULL LIMITS Limits on the maximum pull each anchor would be subjected to were established prior to testing. This limit was established at 2.5 times the anchor's rated working load or holding power, because this is a reasonable margin of safety. Secondly, the ABYC's "Typical Ground Tackle Design Horizontal Loads Table" equates that 63 knots of wind places about 7500 pounds of load on a 50' boat. Finally, preliminary testing of these same anchors at this site, demonstrated that structural damage would occur to some at loads les than 2.5 times their rating. On these anchors, the pull limit was reduced to about 15% less than the load under which damage occurred. Al l the FORTRESS anchors, and Danforth H-1800 were able to withstand pulls of 2.5 their ratings. The Bruce and CQR limits were arbitrarily set at 7,599 lbs. since the manufacturers do not give such ratings. Danforth's Deepset Hi-Tensile T-4000, Standard S-2000 and U.S. Anchor's Sentinel 40 test limits reflect their demonstrated structural strength. TEST PROCEDURE Anchors were scheduled for testing in a revolving order. The anchor to be tested would be attached to it's rode, and staged for deployment at the stern of the tug "Hercules." After the tug had maneuvered into the proper lane and test direction, the standing end of the rode was then attached to the dynometer, and the anchor thrown into the water. The tug would then move forward under minimal power as the rode was payed out. Prior to reaching the end of the rode, the tug was shifted into neutral, allowing it's gentle momentum to drift against the anchor to set it. When a "set" was established: i.e.: when some load was registered upon the dynometer, the transmission was engaged and RPM's slowly increased while the registered loads were carefully obsr3eved and recorded. Loads were then slowly increased until the anchor being tested had either reached it's pre-established test limit and held, "dragged" under constant load, or "pulled out," resulting in the dynometer needle falling to a substantially lower reading as the tug moved through the water. Bearings taken on the nearby seawall established whether an anchor dragged, pulled out, or held. When each test was completed, the standing end of the rode was then disconnected from the dynometer, attached to a buoy, and thrown into the water for recovery by one of the attending workboats. This enabled the next anchor to be tested immediately. using the recovery boat system allowed a new anchor to be tested approximately once every 15 minutes. After each anchor was recovered it was then returned to the tug "Hercules" to he staged for it's next test. TABULATION OF RESULTS When the two days of testing were completed, and the recorded test results compiled, each anchor's performance was then scored and rated into three categories: (1) "Average Test Pull," or, all pulls added up and then divided by the number of pulls to establish an average. (2) "Holding Power Per Pound Of Anchor Weight" sometimes referred to as a "performance ratio" of how many times an anchor's actual weight it is capable of holding in a given bottom, and (3) "Cost Per Pound Of Holding Power" to established useful "value index," based upon advertised list prices divided by the Average Test Pull. The results of these tabulations can be examined in the charts on the next page. A summary of raw test data, as verified by Mr. Maloney and Captain White, is provided on the last page of this report.
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||